| Specifications | |
| Solid Content | 80 ~ 90% |
| Fineness of Grinding (FOG) | <20um |
| Viscosity (Pa-s) | 150 ± 10, Measured with brookfield visco meter HBT - DV3 spindle / chamber SC4-14 / 6R, at 25ºC ± 1ºC |

| Specifications | |
| Solid Content | 50 ~ 60% |
| Fineness of Grinding (FOG) | <20um |
| Viscosity (Pa-s) | 50 +/- 10, Measured with Brookfield visco meter HBT - DV3 spindle / chamber SC4-14 / 6R, at 25ºC ± 1ºC |

| Specifications | |
| Solid Content | 75 ~ 80% |
| Fineness of Grinding (FOG) | <20um |
| Viscosity (Pa-s) | 150 ± 10, Measured with brookfield visco meter HBT - DV3 spindle / chamber SC4-14 / 6R, at 25ºC ± 1ºC |